In: Civil Engineering
A concrete mix is required for reinforced concrete wave breaker at seashore where frequent mild freezing and thawing is dominant. A specified compressive strength of 25 MPa is required at the age of 28 days, and the size of the section and reinforcement dictate using a maximum aggregate size of 19 mm. The company had no history of testing concrete used. The coarse aggregate meets the ASTM grading requirements. It has absorption of 2%, a BSG (D) of 2.70 and a unit weight of 1550 kg/m3. The fine aggregates have absorption of 1%, a BSG (D) of 2.7 and a fineness modulus of 2.7. Both coarse and fine aggregates are used while dry. For each bag of cement (50 kg); calculate the number of containers of coarse and fine aggregate equivalent to required mass quantities. The volume of each container is 20 liters; and the loose density of the coarse and fine aggregates are 1250 and 1200 kg/m3, respectively.
Mix proportions required with complete mix design as per the given specifications is shown below.