A camera film is currently manufactured to a thickness of 25 thousandths. The process engineer wants to increase the speed of the film and believes that this can be achieved by decreasing the film thickness to 20 thousandths. Film speed is measured in µJ / in^2, which is a measure inversely proportional to speed, that is, at higher speed minus µJ / in^2

8 sheets of each thickness are taken (25 mils and 20 mils) and the following results are obtained:

For 25 mils: xbar = 1.15 µJ / in2 and s = 0.11 µJ / in2

For 20 mils: xbar = 1.06 µJ / in2 and s = 0.09 µJ / in2

a) Is there evidence to support the belief of the process engineer? (Assume that σ1 = σ2)

Clearly define the hypothesis, the areas of acceptance and rejection, the test statistic and express your conclusion in complete sentence
b) Calculate the Pvalue for this test

c) Is the presumption of equal variances supported?

Solutions

Expert Solution

◦•●◉✿Solutions✿◉●•◦

◦•●◉✿please✿◉●•◦like


Related Solutions

A camera film is currently manufactured to a thickness of 25 thousandths. The process engineer wants...
A camera film is currently manufactured to a thickness of 25 thousandths. The process engineer wants to increase the speed of the film and believes that this can be achieved by decreasing the film thickness to 20 thousandths. Film speed is measured in µJ / in2, which is a measure inversely proportional to speed, that is, at higher speed minus µJ / in2 8 sheets of each thickness are taken (25 mils and 20 mils) and the following results are...
Problem 6.77. A camera film is currently manufactured to a thickness of 25 thousandths. The process...
Problem 6.77. A camera film is currently manufactured to a thickness of 25 thousandths. The process engineer wants to increase the speed of the film and believes that this can be achieved by decreasing the film thickness to 20 thousandths. Film speed is measured in µJ / in2 which is a measure inversely proportional to speed, that is, at higher speed minus µJ / in2 8 sheets of each thickness are taken (25 thousandths and 20 thousandths) and the following...
A photoconductor film is manufactured at a nominal thickness of 25 mils. The product engineer wishes...
A photoconductor film is manufactured at a nominal thickness of 25 mils. The product engineer wishes to increase the mean speed of the film and believes that this can be achieved by reducing the thickness of the film to 20 mils. Eight samples of each film thickness are manufactured in a pilot production process, and the film speed (in microjoules per square inch) is measured. For the 25-mil film, the sample data result is x1 = 1.15 and s1 =...
A photoconductor film is manufactured at a nominal thickness of 25 mils. The product engineer wishes...
A photoconductor film is manufactured at a nominal thickness of 25 mils. The product engineer wishes to increase the mean speed of the film, and believes that this can be achieved by reducing the thickness of the film to 20 mils. Eight samples of each film thickness are manufactured in a pilot production process, and the film speed (in microjoules per square inch) is measured. For the 25-mil film, the sample data result is x-bar1=1.13 and s1=0.11, while for the...
10.2.8 A photoconductor film is manufactured at a nominal thickness of 25 mils. The product engineer...
10.2.8 A photoconductor film is manufactured at a nominal thickness of 25 mils. The product engineer wishes to increase the mean speed of the film, and believes that this can be achieved by reducing the thickness of the film to 20 mils. Eight samples of each film thickness are manufactured in a pilot production process, and the film speed (in microjoules per square inch) is measured. For the 25-mil film, the sample data result is and while for the 20-mil...
Find the thickness of film of a camera lens coating that minimizes normal reflection in the...
Find the thickness of film of a camera lens coating that minimizes normal reflection in the wavelength range 400 nm to 700 nm. Assume refractive index of film nfilm=1.38 and nglass=1.50
Photo Tonight, a film-developing and camera-repair franchise, began business on January 1, 2020. In the process...
Photo Tonight, a film-developing and camera-repair franchise, began business on January 1, 2020. In the process of beginning operations, it incurred the following capital expenditures: Developing equipment $ 85,000 Furniture and fixtures 35,000 Small tools (under $500) 20,000 Class 14 Franchise (expires in 20 years) 80,000 Incorporation costs 6,000 Pickup truck 14,000 Class 13 Leasehold improvements (10-year lease) 32,000 The business was immediately successful and generated substantial profits for the years ended December 31, 2020 and 2021. In 2021, the...
An investor wants to find the duration of​ a(n) 25​-year, 7​%semiannual​ pay, noncallable bond​ that's currently...
An investor wants to find the duration of​ a(n) 25​-year, 7​%semiannual​ pay, noncallable bond​ that's currently priced in the market at $481.01​, to yield 15​%. Using a 250 basis point change in​ yield, find the effective duration of this bond (Hint​: use Equation​ 11.11). The new price of the bond if the market interest rate decreases by 250 basis points​ (or 2.5​%) is ​$_____. (Round to the nearest​ cent.)
BDJ Co. wants to issue new 25-year bonds for some much-needed expansion projects. The company currently...
BDJ Co. wants to issue new 25-year bonds for some much-needed expansion projects. The company currently has 7.8 percent coupon bonds on the market that sell for $1,125, make semiannual payments, and mature in 25 years. Required: What coupon rate should the company set on its new bonds if it wants them to sell at par? (Do not round intermediate calculations. Round your answer to 2 decimal places (e.g., 32.16).)   Coupon rate %
ADVERTISEMENT
ADVERTISEMENT
ADVERTISEMENT